New try of filling.

First observation: UV glue does not stick on Eppendorf

  • 0.04g agarose + 1.5 ml water ~ 3% solution put in water bath at 70C
  • 0.3 x 0.79 teflon tube into PDMS
  • to fit this tube in Eppendorf needed hole of 0.7-0.8 mm. 18G too large, 23G too smalll, 1mm drill best I could find, but it needs filling in to be pressure tight.
  • Since glue does not stick on Eppendorf or teflon, use glue, but without UV. This will probably be enough for a few mbar pressure.
  • The gel is too viscous and the joints between Eppendorf lid and tubes are leaking.
  • I need a better lid/kork with airtight joints to the tubes.
  • Made a rubber plug with hole for tube. This plug worked well, no leak it seems
  • filling 0.3 mmID teflon tube required more than 100 mbar. When it was filled it flowed at 2 mbar. Hydrophobic capillary
  • outlet (channel 2) must have been plugged. This has to be exchanged every time due to hydrogel plugging
  • apart from this the water (did not use gel this time) filled lamellae and did not go past pillar.